Vinyguard Silvergrey 88 is a quick drying, modified vinyl primer.
As a tie coat or as a sealer for an antifouling system to be compliant with IMO Anti-fouling System Convention (AFS/CONF/26). Can also be used as a primer/touch-up primer under alkyd and acrylic coatings for steel structures.
When used as a sealer coat in 35µm dry film thickness, 5-10% additional thinning may be necessary.
Hong Kong rules: Category of paints - Antifouling sealer coatings; VOC 540 gms/ltr HK EPD method (Ready to use); Exempt compound - N/A; Specific gravity: 1.14;
Both VOC and Specific gravity values provided are typical values, subject to changes when
different colour involved.
*Measured according to ISO 3233:1998 (E)
All surfaces should be clean, dry and free from contamination. The surface should be assessed and treated in accordance with ISO 8504.
Cleanliness: Blast-cleaning to Sa 2½ (ISO-8501-1:2007). Power tool cleaning to min. St 2 (ISO 8501-1:2007) may be acceptable, subject to exposure conditions.
Clean, dry and undamaged approved shopprimer.
Clean, dry and undamaged compatible primer. Contact your local Jotun office for more information.
The coating may be used on other substrates. Please contact your local Jotun office for more information.
The temperature of the substrate should be minimum 3ºC above the dew point of the air, temperature and relative humidity measured in the vicinity of the substrate. Good ventilation is usually required in confined areas to ensure correct drying.
Thinner/Cleaner Jotun Thinner No. 7
Pressure at nozzle 15 MPa (150 kp/cm² 2100 psi)
Nozzle tip 0.46-0.69 mm (0.018-0.027")
Filter Check to ensure that filters are clean.
Drying times are generally related to air circulation, temperature, film thickness and number of coats, and will be affected correspondingly. The figures given in the table are typical with:
Good ventilation (Outdoor exposure or free circulation of air)
Typical film thickness
One coat on top of inert substrate
Substrate temperature |
5°C |
10°C |
23°C |
40°C |
Surface dry |
30 min |
20 min |
15 min |
10 min |
Through dry Dry to recoat, minimum 1 Dry to recoat, maximum 2 |
4h
4h |
3h
3h |
2h
2h |
1.5h
2h |
The given data must be considered as guidelines only. The actual drying time/times before recoating may be shorter or longer, depending on film thickness, ventilation, humidity, underlying paint system, requirement for early handling and mechanical strength etc. A complete system can be described on a system sheet, where all parameters and special conditions could be included.
Below water:
Above water:
Pioner Topcoat 1 x 50 µm (Dry Film Thickness) alternatively
Pilot II 1 x 40 µm (Dry Film Thickness)
Antifouling systems:
See recommendations in the antifouling technical data sheets.
Other systems may be specified, depending on area of use
The product must be stored in accordance with national regulations. Storage conditions are to keep the containers in a dry, cool, well ventilated space and away from source of heat and ignition. Containers must be kept tightly closed.
Handle with care. Stir well before use.
20 litre container
Please observe the precautionary notices displayed on the container. Use under well ventilated conditions. Do not breathe or inhale mist. Avoid skin contact. Spillage on the skin should immediately be removed with suitable cleanser, soap and water. Eyes should be well flushed with water and medical attention sought immediately.